Skip Nav Destination
Close Modal
Search Results for
COLHED
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for COLHED
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
COLHED: Cold Heading Tool Steel, Type W3
Available to Purchase
Alloy Digest (1959) 8 (7): TS-83.
Published: 01 July 1959
... COLHED is a carbon-vanadium tool steel made especially for cold heading dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-83. Producer...
Abstract
View articletitled, <span class="search-highlight">COLHED</span>: Cold Heading Tool Steel, Type W3
View
PDF
for article titled, <span class="search-highlight">COLHED</span>: Cold Heading Tool Steel, Type W3
COLHED is a carbon-vanadium tool steel made especially for cold heading dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-83. Producer or source: Vanadium Alloys Steel Company.