Alloy Digest (2000) 49 (11): Cu-129.
Published: 01 November 2000
... CMW 73 is a heat treatable copper-base alloy having high tensile strength and hardness coupled with fair electrical and thermal conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (2000) 49 (8): Cu-85.
Published: 01 August 2000
... CMW 3 is an age-hardenable copper-base alloy combining high mechanical and electrical properties. The alloy is typically used for spot and seam welding cold and hot-rolled steels and coated materials, current carrying shafts and arms, back-up bars, back-up bars for arc welding, electrical current...