Alloy Digest (2000) 49 (10): Cu-29.
Published: 01 October 2000
... CMW 100 is a copper alloy that combines high tensile strength with high electrical and thermal conductivity. It responds to age-hardening heat treatment. It is used for flash welding dies, springs, electrical components, high-strength backing material for brazed assemblies, and wire guides...
Journal Articles
Alloy Digest (2000) 49 (11): Cu-129.
Published: 01 November 2000
... CMW 73 is a heat treatable copper-base alloy having high tensile strength and hardness coupled with fair electrical and thermal conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (2000) 49 (12): Cu-656.
Published: 01 December 2000
... CMW 353 alloy is a Ni-Si-Cr-Cu high-strength high-conductivity alloy. It has high hardness combined with toughness. This combination gives the alloy excellent wear resistance and makes it useful for flash welding dies, back-up bars, and bushings in current-carrying bearings when used...
Journal Articles
Alloy Digest (2000) 49 (8): Cu-85.
Published: 01 August 2000
... resistance to corrod- ing media as pure copper. Like copper, it is readily attacked by CMW® 3 Filing Code: Cu-85 Copper Revised August 2000 Replaces MALLORY-3 Table 1 Change in Conductivity with Temperature Temperature Electrical conductivity, °C °F %IACS 20 68 80 100 212 61 200 392 47 300 572 41 400 752 33...
Journal Articles
Alloy Digest (2000) 49 (8): W-3.
Published: 01 August 2000
... CMW 3000 is a tungsten-bearing sintered alloy of high density and high strength. It is a powder metallurgical product and one of a series of alloys with densities 50% greater than lead. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (2000) 49 (6): W-2.
Published: 01 June 2000
... CMW 1000, also known as NO-CHAT, is a tungsten bearing sintered alloy of high density and high strength. It is a powder metallurgy product and one of a series of alloys with densities 50% greater than lead. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2001) 50 (6): W-26.
Published: 01 June 2001
... or source: CMW Inc. Producer or Source: CMW Inc. Copyright © ASM International® 2001 2001 ASM International arc erosion resistance bend strength chemical composition ELKONITES TC10 ELKONITES TC20 ELKONITES TC5 ELKONITES TC53 hardness high-temperature alloys joinability oil devices...
Journal Articles
Alloy Digest (2001) 50 (2): W-23.
Published: 01 February 2001
... provides information on composition, physical properties, and hardness. Filing Code: W-23. Producer or source: CMW Inc. Producer or Source: CMW Inc. Copyright © ASM International® 2001 2001 ASM International chemical composition corrosion-resistant alloys ELKONITE 1060 ELKONITE 3042...
Journal Articles
Alloy Digest (1998) 47 (10): SS-713.
Published: 01 October 1998
...- formation, a reduction in magnesium, and more suitability for cold working. Products Available: UGIMA 4570 is available as billets and round CMW bars, un- annealed, softened for cold cutting, tensile strength I850 MPa (123 ksi); wire rod, annealed. tensile strength 1680 MPa; and hot-rolled and cold-finished...
Journal Articles
Alloy Digest (1998) 47 (5): SS-718.
Published: 01 May 1998
... Available: Billets and round constant metric weight (CMW) bars, unannea led soti- ened for cold cutting. tensile strength $850 Mpa 6123 ksi); Wire and rod. annealed, tensile strength &80 Mpa 699 ksi): Hot-rolled and cold-finished bars. Delivery can be annealed. annealed and cold- fin- ished or strain...
Journal Articles
Alloy Digest (1998) 47 (11): SS-734.
Published: 01 November 1998
... (CMW), unannealecl and softened for cold cutting with tensile strength 1850 MPa (123 ksi); wire rod, annealed with tensile strength 1650 MPa (94 ksi). Hot-rolled and cold-finished bars are supplied in the annealed (solution treated) condition that enables resistance to intergtanu- lar corrosion...
Journal Articles
Alloy Digest (1998) 47 (12): SS-735.
Published: 01 December 1998
... to be preferred over type 316 for applications involving welding during fabrication This grade complies to EC 9497 directive on Ni-release requirement. Products Available: Billets and round constant metric weight (CMW), uuannea.led and sof- tened fa cold cutting with tensile strength 5850 MPa (123 ksi). Wire rod...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-449.
Published: 01 December 1982
... Density, Ib/cu in. (At 68°F) Specific gravity Melting point, T (Solidus-Liquidus) Oc (Solidus-Liquidus) Specific heat, Btu/lb/ F (At 77°F) Thermal coef. expansion/OF (68-572°F) PC 2&3ooq Thermal conductivity, 1 Btu/ft /ft/br/OF (At 68°F) cal/cm2/cmW°C (At UPC) Electrical conductivity,*t 070 LACS (At 68°F...