1-7 of 7 Search Results for

CMSX-3

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1993) 42 (1): Ni-420.
Published: 01 January 1993
... CMSX-3 is a single crystal alloy development of Cannon-Muskegon Corporation designed to achieve a balance in properties at high temperatures. This datasheet provides information on composition and physical properties as well as creep. It also includes information on corrosion resistance. Filing...
Journal Articles
Alloy Digest (1998) 47 (2): Ni-537.
Published: 01 February 1998
... heat treatments, and provides creep strength that is as good or better than other first generation SX materials such as CMSX-2 (Alloy Digest Ni-417, November 1992), CMSX-3 (Alloy Digest Ni-420, January 1993), CMSX-4 (Alloy Digest Ni-447, March 1994), CMSX-6 (Alloy Digest Ni-418, December 1992), PWA...
Journal Articles
Alloy Digest (1994) 43 (3): Ni-447.
Published: 01 March 1994
... CMSX-4 ALLOY is a good second generation single crystal superalloy containing 3% Re. It has been extensively developed to maximize overall properties, through collaborative programs with several turbine engine companies, involving over one hundred 400 lb. (182 kg) and several 8000 lb. (3630 kg...
Journal Articles
Alloy Digest (1998) 47 (1): Ni-533.
Published: 01 January 1998
... and 36 ksi) when compared to CMSX-4. CMSX-3 (Alloy Digesr Ni-417). DS CM 186 LC (Alloy Digest Ni-450). and DS CM 247 LC (Alloy Digest Ni-415) alloys. The CMSX-10 ahoy exhibits advantages in time to 1% creep of 4.6 to 80 times that of the comparative materials. Heat Treatment: The CMSX-10 ahoy contains...
Journal Articles
Alloy Digest (1994) 43 (4): Ni-450.
Published: 01 April 1994
... LONGITUDINAL CM 186 LC@ vs. CM 247 LC@ vs. CMSX-2/3@ (001) I / - -~roo1, 96soh.+snglsmacwubkAgs 1.6 mm - 6.4 mm do SdlQs 69Dmapoinb .OSLonglludiMlA~ -SUWSdll+DOdS&P 32mn-4.1mm&aSdkk 26DaaPcdlt3 LibRaf~~e42-624hfS 3.2mm-4.5mtsaSows 2oDamPoilns l Ulelange47-732hrs 40 42 52 54 56 56 DOI: 10.31399/asm.ad.ni0450...
Journal Articles
Alloy Digest (1992) 41 (12): Ni-418.
Published: 01 December 1992
... alloy development to retrofit existing turbine designs. CMSX-6@ alloy is a registered trademark of Cannon-Muskegon Corporation. Composition, Wt. %: Physical Constants: Chromium 10 Density, lb/cu in. (kg/cu dm) Cobalt 5 Molybdenum 3 Titanium 4.7 Aluminum 4.8 Tantalum 2 Hafnium 0.1 Nickel Bal. PROPERTIES...
Journal Articles
Alloy Digest (1992) 41 (11): Ni-417.
Published: 01 November 1992
... superalloys (gas velocity Mach 1, thermal cycles of one hour followed by rapid cooling.) t METALLOSSPERSlDE(mm) 1.6 t / DSMARM t 200Hf 2075°F 50 100 150 200 250 Time(h) Produceabllity and Results: CMSX-2@ alloy is at full production status. Many 8000 lb (3630kg) V-3 furnace heats have been melted...