Alloy Digest (2007) 56 (6): SS-991.
Published: 01 June 2007
... International chemical composition CLC 18-10 Nb creep properties ductility elasticity fracture toughness joinability machinability physical properties shear strength tensile properties workability thermal properties UNS S34700 Chemical Composition, wt (Typical) Carbon 0.030 Chromium 17.5...