Alloy Digest (2014) 63 (6): SS-1176.
Published: 01 June 2014
... CLC 1.2316 is a prehardened mold steel with improved corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1176...
Journal Articles
Alloy Digest (2014) 63 (7): SS-1177.
Published: 01 July 2014
... CLC 1.2316S is a prehardened mold steel with improved corrosion resistance. Sulfur is added for machinability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...