Alloy Digest (2005) 54 (1): TS-611.
Published: 01 January 2005
... CLC 1.2311 is a prehardened mold steel optimized for martensite and surface finish quality. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low...
Journal Articles
Alloy Digest (2005) 54 (2): TS-613.
Published: 01 February 2005
..., but the conditions used for CLC 1.2311 could be applied taking into account a 30% increase in milling speed with carbide inserts, and a 300% increase in drilling speed with high-speed steel tools. Polishability: CLC 1.2312 can be roughly polished in the quenched-and- tempered condition. After grinding, polishing...