Alloy Digest (1959) 8 (4): TS-81.
Published: 01 April 1959
... CHW is a high tungsten hot work steel having highest hardness and good wear resistance. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code...