Alloy Digest (1981) 30 (12): TS-392.
Published: 01 December 1981
... CHROMEWEAR 300 is an air-hardening tool steel developed for applications that require extremely high abrasion resistance. It far exceeds the wear-resistance properties of the air-hardening high-carbon high-chromium steels, and is even superior in wear resistance to the high wear-resistant AISI...