Publisher: Journals Gateway
Alloy Digest (1977) 26 (10): Cu-341.
Published: 01 October 1977
... CHASE 14310 is a high-conductivity copper with excellent resistance to thermal softening. It is a deoxidized, electronic grade of copper with excellent formability, weldability and plateability. It is available in strip form and has a wide range of applications. This datasheet provides information...