Alloy Digest (1978) 27 (8): Bi-6.
Published: 01 August 1978
... CERROBEND Alloy is a bismuth-base eutectic alloy that melts at 158 F (70 C). It is low melting temperature and controlled-shrinkage characteristics make it highly useful industry for such applications as anchoring bushings in drill jigs, cores for spinning and tube-bending filler. This datasheet...
Journal Articles
Alloy Digest (1981) 30 (1): Bi-21.
Published: 01 January 1981
... CERROLOW-147 Alloy is a bismuth-base non-eutectic alloy that melts over the narrow, low-temperature range of 142-149 F (61-65 C). It has a slightly lower melting temperature than CERROBEND Alloy (Alloy Digest Bi-6, August 1978) and functions about as well for the same uses if its small freezing...