Alloy Digest (1991) 40 (6): P-28.
Published: 01 June 1991
... CELANESE Nylon 1100 is an intermediate molecular weight grade for extrusion into monofilaments. CELANESE Nylon 1200 is a high molecular weight grade for extrusion. CELANESE Nylon 1200N-186 is a heat stabilized version of Celanese Nylon 1200 grade. This datasheet provides information on physical...