Alloy Digest (1991) 40 (7): Cu-562.
Published: 01 July 1991
... CBX CUPRON ALLOY is a resistance alloy with practically constant resistance over the range of -67 to 221 F. The alloy does not generate gas when in contact with glass, enamel or ceramic type materials, an advantage over CB CUPRON (Constantan). This datasheet provides information on composition...