Alloy Digest (1980) 29 (12): TS-374.
Published: 01 December 1980
... CARPENTER STAR MAX is a general-purpose, molybdenum-bearing, high-speed steel containing a low percentage of tungsten. It is produced by the ESR (Electroslag Refining) process to provide a cutting steel with as great a toughness as any other high-speed steel. Star Max can be used successfully...