1-1 of 1 Search Results for

CARPENTER STAINLESS TYPE 440F

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (8): SS-449.
Published: 01 August 1984
... CARPENTER STAINLESS TYPE 440F is a high-carbon chromium steel designed to provide stainless properties with maximum hardness. It is free-machining, easy to grind and polish, and has certain nongalling and noseizing properties in metal-to-metal contact. After austenitizing and quenching in oil...