Published: 01 October 1984
... CARPENTER STAINLESS TYPE 440A is a high-carbon chromium steel designed to provide stainless properties at high hardness. It has sufficient corrosion resistance in the annealed condition to permit its use in mild environments. In some respects it behaves similarly to tool steels. It can be...