Alloy Digest (1974) 23 (7): SS-298.
Published: 01 July 1974
... CARPENTER STAINLESS No. 7-Mo is a two-phase alloy consisting of a ferritic matrix with pools of austenite. It has high resistance to stress-corrosion cracking and pitting, and good general corrosion resistance in many environments. Its principal use is for tubing and pipe in heat exchangers...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (9): SS-608.
Published: 01 September 1995
... CARPENTER 7-Mo PLUS is a duplex stainless steel of austenite in a ferrite matrix. It is superior to 300 series stainless steels like types 304 and 316 in strength, corrosion, pitting and stress-corrosion cracking resistance (to chlorides). Typical applications are heat exchangers in the chemical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (11): SS-477.
Published: 01 November 1986
... CARPENTER PH 13-8 Mo is a martensitic precipitation-hardening stainless steel. It has high strength and hardness combined with good ductility and toughness in large sections. Compared to other ferrous alloys this material offers a high level of useful mechanical properties under severe...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (5): SS-716.
Published: 01 May 1998
... 455 stainless or PH 13-8 MO* stain- IeSS. Forms Available: Billef bar. wire, strip Producer: Carpenter Technology Corporation Reading. PA 19612 (610) 2082000 (800) 6546543 ISSN: 002-614X SS-7 168 Table 4 Typical Room Temperature Mechanical Properties of Rod Product 0314 n2 112 951 138 20 75 29.5 H9w...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (12): Ni-133.
Published: 01 December 1997
... trademark of Westinghouse El&c Cotporation Carpenter and HyMu 80 aUoy are trademarksofczarpenter T&logy Corp.- Chemical Composition, wL%: Physical Properties: tkRSilY.kehdm31 speifice 8746 (03 la) 8.14 31.4Cl8.1) 1450 (2642) 0.6 (MO) CnriemrpasmrrTm 4600 cDefiiciandTupto538T 0.00 11(0.ooo6) @EPF~~IO lOWoF...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (9): SS-47.
Published: 01 September 1956
... Code: SW7 CARPENTER STAINLESS Stainless Steel No. 2 8, No. 2-FM SEPTEMER 1956 - DATA ON WORLD WIDE METALS AND ALLOYS PnblizbJ by Engintig AIIoys Digest, Inc Upper MO&, New Jersey CARPENTER STAINLESS No. 2 & No. 2-FM (Stainless Steel Type 420 & 420-F) CARPENTER STAINLESS No. 2 is a high carbon hear...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (7): Ni-556.
Published: 01 July 1999
.... To demonstrate the resistance of 20Mo-6 HS stainless to significant ductility loss as a result of strain aging, cold-drawn armor- ing wire products were given simulated well-age treatments and then subsequently were wrap tested. Results are shown in Tables 6 and 7. Weldability: 20Mo-6 HS stainless can be readily...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (11): SS-63.
Published: 01 November 1957
... CARPENTER STAINLESS No. 20 and No. 20-Cb are wrought low carbon austenitic alloy steels of high nickel and chromium content. They are highly resistant to hot and cold strong acids. No. 20-Cb contains columbium for carbide stabilization and retention of its corrosion resistance in the as-welded...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (8): SS-1325.
Published: 01 August 2020
... Technology Corporation CarTech 25Ni-20Cr-6Mo ASTM UNS N08926 EN X1NiCrMoCuN25 20 7 (1.4529) ISO X1NiCrMoCuN25-20-7 (4529-089-26-I) VDM Metals GmbH VDM Alloy 926 (Cronifer 1925 hMo) General Characteristics Higher strength than Type 904L stainless steel, excellent general corrosion resistance when in contact...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (6): SS-596.
Published: 01 June 1995
... be used to prevent glazing. For more ckaikd machining recommendations for Type 316L stain- less, consult the Guide to Machining Carpenter Stainless Steel and Specialty Metals, available from the producer. Die Threading Tawing Milling, End-Peripheral Broaching Threads 3 to 7-l/2 SFPM 8-15 Per 8-15 SPPM...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (1): SS-915.
Published: 01 January 2005
... BioDur 734 is a nitrogen-strengthened, austenitic stainless steel. The alloy exhibits improved tensile strength, impact strength, fatigue strength, and crevice and pitting corrosion resistance over standard Type 316L. The microstructural integrity and cleanness of this alloy are ensured through...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (12): SS-22.
Published: 01 December 1954
... elasticity fracture toughness hardness heat treatability high-temperature alloys joinability physical properties tensile properties USS 5 USS 5S workability 1 0 r DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS uss 5 Filing Code: 55122 Stainless Steel DECEMBER 1954 (Corrosion and Heat Resisting...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (8): SS-757.
Published: 01 August 1999
...-Free High-Nitrogen Austenitic Stainless Steel Alloy) BioDur 108 alloy is an austenitic alloy but is essentially nickel-free. It contains a very high content of nitrogen to maintain the austenitic struc- ture. The major uses for this alloy are in the biochemical industry for products such as implantable...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (10): SS-19.
Published: 01 October 1954
... Uniloy 19-9DL workability Filing Code: SS-19 UNILOY 19-9DL Stainless Steel OCTOBER, 1954 - DATA ON WORLD WIDE METALS AND ALLOYS . .Poblirbd@ UNlLOY 19-9DL is a chromium-nickel at least 1200 deg. F. Composition: UNILOY 19.9DL Physkal constants Carbon 018-0.X !i!sr= 0.75-1.50 sP=+ gc4vicy, g/cc m. 0.30...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1962) 11 (1): TS-113.
Published: 01 January 1962
... Temperature OF (Harrs) Rockwell C Hardness (by conversion) 5 512-532 : 477-495 44 61 : 418-430 5 ::z: : : 467-477 430-444 : 402-418 351-364 53.0 49.8 47.5 44.5 40.0 35.2 55.0 51.0 48.7 46.5 43.7 38.5 532 495 555 512 460 418 402 52.8 532 ii:: 460 18 36.4 4 7 ;: 54.7 555 51.0 495 47.5 444 43.0 402 37.6 375...