Alloy Digest (1988) 37 (12): TS-494.
Published: 01 December 1988
... CARPENTER SOLAR alloy is an extremely tough, water-hardening tool steel. Large sections harden to a hard case with a tough core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1991) 40 (9): TS-32.
Published: 01 September 1991
.... It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-32. Producer or source: Carpenter. Originally published as Solar, April 1955, revised September 1991. Producer or Source: Carpenter Copyright ┬ę ASM International┬« 1996 1996 ASM International...