1-5 of 5 Search Results for

CARPENTER PROJECT 70 CUSTOM 630

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2003) 52 (6): SS-886.
Published: 01 June 2003
... Carpenter Project 70+ Custom 630 is a modified version of conventional stainless steel Type 630 (17Cr-4Ni) with improved machinability. The alloy has good fabrication characteristics and can be age hardened by a single-step, low-temperature treatment. See also Carpenter Custom 630, Alloy Digest SS...
Journal Articles
Alloy Digest (1998) 47 (11): SS-732.
Published: 01 November 1998
... Carpenter Project 70 Stainless Custom 630 is a modified version of type 630 stainless steel with improved machinability when compared to conventional type 630. The alloy is a martensitic precipitation, age-hardening stainless steel offering high strength and hardness along with excellent corrosion...
Journal Articles
Alloy Digest (2000) 49 (5): SS-788.
Published: 01 May 2000
... Carpenter Project 7000 15Cr-5Ni offers strength and excellent corrosion resistance. Similar to Carpenter 15Cr-5Ni (Alloy Digest SS-346, January 1978) and Carpenter Custom 630 (Alloy Digest SS-258, revised December 2000), Project 7000 15Cr-5Ni stainless is intended for use when improved machining...
Journal Articles
Alloy Digest (2000) 49 (12): SS-258.
Published: 01 December 2000
...-temperature treatment. Manufacturers interested in real- izing the potential economic benefits and lower costs associated with higher machining speeds and lower cycle times should consider this alloy in the Project 70 version. Customers have reported that this alloy offers significantly improved machinability...
Journal Articles
Alloy Digest (2003) 52 (7): SS-889.
Published: 01 July 2003
... Carpenter Project 70+ 15Cr-5Ni is a modified version of Type 15Cr-5Ni stainless steel with improved machinability. The material meets all aspects of the aerospace specification AMS 5659. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile...