1-3 of 3 Search Results for

CARPENTER PCLW-B

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2015) 64 (10): Cu-842.
Published: 01 October 2015
.... Producer or Source: Carpenter Specialty Wire Products Copyright © ASM International® 2015 2015 ASM International CARPENTER PCLW-B chemical composition extension wire physical properties tensile properties workability thermal properties Carpenter PCLW-BPX alloy is a copper-base positive...
Journal Articles
Alloy Digest (1992) 41 (1): Cu-568.
Published: 01 January 1992
... range of applica- tion is 0-200°C (32-392OF). PCLW-BPX is a copper-base positive extension wire used with copper as the negative leg for compensating exten- sion wires for ISA Type B (platinum, 30% rhodium vs platinum, 6% rhodium thermocoupies. PCLW-BPX Al- loy vs copper produces a maximum error of f38...
Journal Articles
Alloy Digest (2012) 61 (2): Cu-803.
Published: 01 February 2012
.... Producer or source: Carpenter Technology Corporation. Producer or Source: Carpenter Technology Corporation Copyright © ASM International® 2012 2012 ASM International CARPENTER PCLW-SNX ALLOY chemical composition physical properties tensile properties thermocouples workability thermal...