Alloy Digest (1980) 29 (8): TS-368.
Published: 01 August 1980
... CARPENTER No. 408 Punch Steel was developed specifically to meet the needs of the pharmaceutical industry. It has the necessary wear resistance to withstand the severe conditions of handling the abrasive materials that must be pellitized. It also has high strength in combination with excellent...