Alloy Digest (1987) 36 (2): SA-423.
Published: 01 February 1987
... CARPENTER NIMARK 300 is a vacuum-melted, low-carbon nickel-cobalt-molybdenum maraging steel that develops yield strengths in excess of 270,000 psi (1862 MPa) by simple low-temperature aging at 900 F (482 C) following a solution anneal. It is readily weldable and exhibits good ductility at high...
Journal Articles
Alloy Digest (1970) 19 (7): SA-254.
Published: 01 July 1970
... NIMARK 300 is a vacuum melted low carbon, 18% nickel alloy steel which attains yield strengths in excess of 270,000 psi. It is recommended for high strength, shock resisting applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1986) 35 (4): SA-417.
Published: 01 April 1986
... CARPENTER NIMARK 250 is a vacuum-melted, low-carbon nickel-cobalt-molybdenum maraging steel in which yield strengths in excess of 240,000 psi can be developed by a simple aging treatment following a solution anneal. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1965) 14 (5): SA-177.
Published: 01 May 1965
... NiMark I is a vacuum melted low-carbon alloy steel in which yield strengths in excess of 240,000 psi can be developed. It is readily weldable and exhibits good ductility at high strength levels. This datasheet provides information on composition, physical properties, hardness, and tensile...