Alloy Digest (1986) 35 (8): Ni-338.
Published: 01 August 1986
... CARPENTER NICKEL-COPPER ALLOY 405 is the free-machining grade of Carpenter Nickel-Copper Alloy 400, the result of a controlled amount of added sulfur. Like Alloy 400, Alloy 405 is a solid-solution alloy and therefore strengthed only by cold work. Its strength is comparable to that of structural...