Alloy Digest (2005) 54 (11): TS-622.
Published: 01 November 2005
... information on forming and heat treating. Filing Code: TS-622. Producer or source: Carpenter Specialty Alloys. Producer or Source: Carpenter Specialty Alloys Copyright © ASM International® 2005 2005 ASM International CARPENTER MICRO-MELT M48 chemical composition die inserts elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (5): SS-884.
Published: 01 May 2003
.../asm.ad.ss0884 Table 2 Typical Machining Speeds and Feeds Tool material Speed, fpm Feed, ipr Tool material Speed, fpm Feed, ipr Turning, single-point and box tools Micro-Melt Powder HS, M48, T15 Depth of cut, in., 0.150 171 0.0180 Depth of cut, in., 0.025 202 0.0084 Carbide C2, uncoated, depth of cut, in., 0.150...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (4): SS-882.
Published: 01 April 2003
... 75 55 68 50 704 1300 517 75 655 95 21 60 187 92 HRB 108 80 102 75 25.4 mm (1 in.) round bar, hardened at 982 °C (1800 °F) 1/2 hour, oil quenched and tempered 2 h Rough reaming (continued) Micro-Melt Powder HS, M48, T15 (continued) Table 2 Typical Machining Speeds and Feeds Tool material Speed, fpm...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (2): SS-875.
Published: 01 February 2003
... Feed, ipr Tool material Speed, fpm Feed, ipr Turning, single-point and box tools Micro-Melt Powder HS, M48, T15 Depth of cut 0.150 in. 140 0.0180 Depth of cut 0.025 in. 171 0.0084 Carbide C2, uncoated, depth of cut 0.150 in. 470 0.0180 Carbide C2, coated, depth of cut 0.150 in. 600 0.0180 Carbide C3...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (6): SS-886.
Published: 01 June 2003
... Speeds and Feeds for Turning with Single-Point and Box Tools Tool material Depth of cut, in. Speed, fpm Feed, ipr Tool material Depth of cut, in. Speed, fpm Feed, ipr Solution-treated or double-aged H1150-M Micro-Melt Powder HS M48, T15 0.150 90 0.015 0.025 105 0.007 Carbide C6, uncoated 0.150 375 0.015...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (3): SS-878.
Published: 01 March 2003
...: Carpenter Specialty Alloys Reading, PA 19612 (610) 208-2000 (800) 654-6543 ISSN: 002-614X SS-878B Table 3 Typical Machining Speeds and Feeds Tool material Speed, fpm Feed, ipr Tool material Speed, fpm Feed, ipr Turning, single-point and box tools Micro-Melt Powder HS, M48, T15 Depth of cut, in., 0.150 140...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (11): TS-546.
Published: 01 November 1996
... or subcritically anneal the hot workpiece after forging. Subsequent full annealing of workpiece should occur prior to hardening. Specification Equivalents: AlSl Type M48 UNS Type T11348 DOI: 10.31399/asm.ad.ts0546 Table 1 Effect of Hardening and Tempering Temperature on Hardness of Carpenter Micro-Melt HS-76 Alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (10): SS-979.
Published: 01 October 2006
.../16 140 0.0005 1/8 140 0.002 ¼ 140 0.004 ½ 140 0.006 ¾ 140 0.0077 1 140 0.0088 1½ 140 0.0098 2 140 0.0098 Table 1(c) Typical Machining Speeds and Feeds Rough Reaming Tool material Reamer diameter, in. Speed, fpm Feed, ipr M48, T15 Micro-Melt 1/8 72 0.003 powder high speed ¼ 72 0.005 ½ 72 0.008 1 72...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (7): SS-889.
Published: 01 July 2003
... Table 2 Typical Machining Speeds and Feeds for Turning with Single-Point and Box Tools Tool material Depth of cut, in. Speed, fpm Feed, ipr Solution-treated material Micro-Melt Powder HS, M48, T15 0.150 85 0.015 0.025 100 0.010 Carbide C6, uncoated 0.150 340 0.019 Carbide C6, coated 0.150 440 0.019...