1-10 of 10 Search Results for

CARPENTER HS 50

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2004) 53 (6): Fe-130.
Published: 01 June 2004
... traces of oil from the parts. The temperature of the furnace can then be slowly raised until the load reaches 760 °C (1400 °F). The tem- perature should be held within ±10 °C (±18 °F) for 2 h before cooling at CARPENTER HS 50 Filing Code: Fe-130 Iron June 2004 CARPENTER HS 50 (Cobalt-Iron Soft-Magnetic...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-556.
Published: 01 July 1999
... Carpenter 20Mo-6 HS is an alloy in the generic family of 6% molybdenum alloys, which are very corrosion resistant. This steel also possesses an excellent resistance to environmental cracking. (See also Carpenter 20Mo-6, Alloy Digest SS-444, May 1984.) This datasheet provides information on...
Journal Articles
Alloy Digest (1998) 47 (8): Fe-118.
Published: 01 August 1998
... forging. the piece can be air cooled. Table 1 Magnetic Properties of Hipewx Alloy 27 HS WW-w4H Ml@tSkiUdIdO&B Ah oe T c 2.387 30 1.55 15500 3.979 50 I .8 18,000 7.958 100 2.0 20,ooo 11.937 150 2.1 2l.ooo 15.915 200 2.15 2l.500 Typical nlagnenc lIducIion of forged bar after being armaled at 760 C ( 1400T...
Journal Articles
Alloy Digest (2003) 52 (4): SS-882.
Published: 01 April 2003
... 75 55 68 50 704 1300 517 75 655 95 21 60 187 92 HRB 108 80 102 75 25.4 mm (1 in.) round bar, hardened at 982 °C (1800 °F) 1/2 hour, oil quenched and tempered 2 h Rough reaming (continued) Micro-Melt Powder HS, M48, T15 (continued) Table 2 Typical Machining Speeds and Feeds Tool material Speed, fpm...
Journal Articles
Alloy Digest (2003) 52 (5): SS-884.
Published: 01 May 2003
... temperature, 25.4 mm (1 in.) round bar, annealed at 1038 °C, or 1900 °F.) Modulus of elasticity in tension, 193 (28.0) GPa (106 psi) Yield strength, 0.2%, MPa (ksi) 241 (35) Tensile strength, MPa (ksi) 621 (90) Elongation in 50.8 mm (2 in % 50 Reduction of area, % 55 Hardness, HB 160 Impact strength, J (ft...
Journal Articles
Alloy Digest (2003) 52 (6): SS-886.
Published: 01 June 2003
... Speeds and Feeds for Turning with Single-Point and Box Tools Tool material Depth of cut, in. Speed, fpm Feed, ipr Tool material Depth of cut, in. Speed, fpm Feed, ipr Solution-treated or double-aged H1150-M Micro-Melt Powder HS M48, T15 0.150 90 0.015 0.025 105 0.007 Carbide C6, uncoated 0.150 375 0.015...
Journal Articles
Alloy Digest (2003) 52 (3): SS-878.
Published: 01 March 2003
... Characteristics: Project 70+ Type 316/316L stainless is an improved-machining version of conventional Type 316/316L stainless and replaces Project 70 and Project 7000 alloys of the same grade. (See Alloy Digest SS-339 and SS-515.) Users may be able to attain machining-speed improvements of up to 50% and higher...
Journal Articles
Alloy Digest (2003) 52 (2): SS-875.
Published: 01 February 2003
... 70 and Project 7000 alloys of the same grade (see Alloy Digest SS-418 and SS-513). Users may be able to attain machining speed improvements of up to 50% and high- er over AISI Type 304/304L. This material has been designed to reduce tool wear and increase machine speeds and feeds to help improve...
Journal Articles
Alloy Digest (2003) 52 (7): SS-889.
Published: 01 July 2003
... precipitation-hardenable stainless steels. The reduction in toughness can be minimized in some cases by using higher aging temperatures. Short exposures to elevated temperatures can be con- sidered, providing the maximum temperature is at least 28 °C (50 °F) less than the aging temperature. Product Forms...
Journal Articles
Alloy Digest (1998) 47 (6): Co-105.
Published: 01 June 1998
... kminations using ASTM Method A 596/A S%M. For a given strength level, the flux density is in- dependent of strip thickness. General Characteristics: Hiperco 50 HS is an iron-cobalt-vanadium soft magnetic alloy that exhibits high magnetic sauuation (24 kilogauss) and a unique combination of high yield...