Journal Articles
Alloy Digest (1997) 46 (12): Ni-133.
Published: 01 December 1997
..., elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ni-133. Producer or source: Carpenter. Originally published as Hipernom, May 1968, revised December 1997. Producer or Source: Carpenter Copyright ┬ę ASM International┬« 1997...
Journal Articles
Alloy Digest (1989) 38 (10): Ni-375.
Published: 01 October 1989
.... *HyMu 80 and HIPERNOM are registered trademarks of Carpenter Technology Corp. Composition: Carbon Manganese Silicon Molybdenum Nickel Iron Type Analysis 0.02 0.50 0.35 4.20 80.00 Remainder Table 1 -MEAN COEFFICIENT OF THERMAL EXPANSION Temperature Coefficient Range of Expansion OF lO+F -103 to 77 6.0...