Alloy Digest (1988) 37 (2): Co-83.
Published: 01 February 1988
... CARPENTER HIPERCO 50 is a magnetic soft alloy used primarily as magnetic core in electrical equipment requiring high permeability at very high magnetic flux densities. These magnetic characteristics permit weight reduction, reduction of copper turns and insulation in the end product in comparison...
Journal Articles
Alloy Digest (1998) 47 (6): Co-105.
Published: 01 June 1998
... Hiperco 50HS is an improved soft magnetic alloy with a finer grain size that produces greater strengths than those found in Hiperco 50 (Alloy Digest Co-83, February 1988). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1998) 47 (8): Fe-118.
Published: 01 August 1998
... properties, and tensile properties. It also includes information on forming and heat treating. Filing Code: FE-118. Producer or source: Carpenter. Producer or Source: Carpenter Copyright © ASM International® 1998 1998 ASM International chemical composition heat treatability Hiperco Alloy 27 HS...
Journal Articles
Alloy Digest (2002) 51 (10): Fe-124.
Published: 01 October 2002
... the advan- tages of high-saturation magnetization (compared to silicon-iron, pure iron), high electrical resistivity (compared to Hiperco Alloy 27, pure iron), and lower cobalt content (compared to Hiperco Alloy 50 and Hiperco Alloy 27). Product Forms Available: Strip, bar, and billet are available...
Journal Articles
Alloy Digest (1999) 48 (11): Co-107.
Published: 01 November 1999
... to those of other com- mercial iron-cobalt soft magnetic alloys. Carpenter Technology Corporation also produces Hiperco 50 (see Alloy Digest Co-50), which has nearly the same nominal analysis as Hiperco 50A but contains small additions of nio- bium and carbon for grain refinement to achieve higher me...