Alloy Digest (1998) 47 (5): SS-716.
Published: 01 May 1998
... Carpenter Custom 465 stainless steel is an age-hardenable martensitic alloy with less sensitivity to process parameters than other similar alloys. It develops high strength along with fracture toughness and resistance to stress-corrosion cracking. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2012) 61 (3): SS-1117.
Published: 01 March 2012
... Micro-Melt BioDur Custom 470 stainless is a powder metallurgy-based improved-machining version of Custom 465 stainless steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming and heat...