Alloy Digest (2013) 62 (9): SS-1155.
Published: 01 September 2013
... Carpenter CTS-B90 alloy is a high-carbon, chromium-molybdenum-vanadium martensitic stainless steel that provides high hardness and wear resistance. This alloy attains a hardness of up to HRC 57/59 when heat treated and is used for knives, cutting tools, and bearing applications. This datasheet...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1188.
Published: 01 November 2014
... alloy, like all high carbon tool steels, is subject to decarburization during thermal processing, and precautions must be taken to control this condition. Annealing. CTS-B90 alloy should be annealed in a neutral atmosphere. Heat uniformly to 816 899 °C (1500 1650 °F), then cool very slowly in the...
Journal Articles
Alloy Digest (1954) 3 (7): Cu-18.
Published: 01 July 1954
... PROPERTIES Tensile streng& psi yield strengrh (02%) psi Elongation, % in 2 Ro&wellhardness Ekcrrical conductiviy, 7. 1A.C.S. As-cast 70,000 min. 40,000 min. 15 min. B75 min. 15 mirL cast& Heat Treated 85,000 min. 45,000 min. 15 min. B90 min. 18 min. sOlUdoll Annealed % Water Quenched 55,000 max. 20,000 max...