Journal Articles
Alloy Digest (1979) 28 (11): SS-370.
Published: 01 November 1979
... CARPENTER CRB-7 is a corrosion-resistant, wear-resistant and secondary-hardening steel for high-temperature bearings. It has high quenched-and-tempered hardness and maintains high hardness at elevated temperatures. CRB-7 is a martensitic type of stainless steel. This datasheet provides information...