Skip Nav Destination
Close Modal
Search Results for
CARPENTER BARTO
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for CARPENTER BARTO
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1985) 34 (7): TS-444.
Published: 01 July 1985
... CARPENTER BARTO is a cold-melt, grain-controlled, electric-furnace chromium-nickel tool steel. It was developed for applications requiring extreme toughness. Barto's extreme toughness is developed at the expense of some wear resistance; however, it will harden to Rockwell C 55/56. Typical...
Abstract
View articletitled, <span class="search-highlight">CARPENTER</span> <span class="search-highlight">BARTO</span>: Chromium Nickel Tool Steel
View
PDF
for article titled, <span class="search-highlight">CARPENTER</span> <span class="search-highlight">BARTO</span>: Chromium Nickel Tool Steel
CARPENTER BARTO is a cold-melt, grain-controlled, electric-furnace chromium-nickel tool steel. It was developed for applications requiring extreme toughness. Barto's extreme toughness is developed at the expense of some wear resistance; however, it will harden to Rockwell C 55/56. Typical applications are clutch parts and expander punches. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-444. Producer or source: Carpenter.