Journal Articles
Alloy Digest (1994) 43 (7): TS-529.
Published: 01 July 1994
... CARPENTER 883 PLUS is a 5% Chromium hot work die steel designed for applications requiring both toughness and good red-hardness. It achieves this with higher purity, homogeneity and greater structural integrity than standard AISI type H13. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1987) 36 (1): TS-469.
Published: 01 January 1987
... CARPENTER 883 PLUS is a premium quality die-casting die steel. It is electroslag remelted and this together with processing adaptations give it metallurgical consistency and improved isotropic properties. This datasheet provides information on composition, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1971) 20 (1): Ti-61.
Published: 01 January 1971
... the standpoint of optimum mechanical properties. Machinability: Rigid set-ups, good coolants and slow speeds are necessary for all machining operations on CARPENTER TITANIUM 66-2 Efficient and successful machining depends on tool life. Turning: Carbide tools such as K6, 883, and HA are recommended. High speed...
Journal Articles
Alloy Digest (2000) 49 (12): SS-258.
Published: 01 December 2000
... Carpenter Custom 630 is a martensitic precipitation (age) hardening (PH) stainless steel offering high strength and hardness along with excellent corrosion resistance. It has good fabricating characteristics and can be age hardened by a single-step, low-temperature treatment. This datasheet...
Journal Articles
Alloy Digest (1978) 27 (7): SS-353.
Published: 01 July 1978
... of IO-15 volume percent nitric acid plus 1-2 percent hydrofluoric acid at 100/130oF (38/54oC) for lo-15 minutes or until clean. Water rinse and immerse in 20 volume percent nitric acid at room temperature for 5 minutes and water rinse. Carpenter 22Cr-13Ni-5Mn is Grade XM19 in the following ASTM...
Journal Articles
Alloy Digest (2000) 49 (5): SS-788.
Published: 01 May 2000
... Carpenter Project 7000 15Cr-5Ni offers strength and excellent corrosion resistance. Similar to Carpenter 15Cr-5Ni (Alloy Digest SS-346, January 1978) and Carpenter Custom 630 (Alloy Digest SS-258, revised December 2000), Project 7000 15Cr-5Ni stainless is intended for use when improved machining...