Alloy Digest (1977) 26 (3): SS-337.
Published: 01 March 1977
... Carpenter 430FR Solenoid Quality stainless steel is a ferritic chromium-iron alloy developed especially for A.C. and D.C. magnetic circuit applications such as solenoid valve core components and electromagnetic relay cores. The electrical resistivity of 430FR is approximately 25% higher than other...
Journal Articles
Alloy Digest (1998) 47 (6): SS-720.
Published: 01 June 1998
... Carpenter Chrome Core 18-FM solenoid quality stainless was developed with optimal corrosion resistance in mind. The result was an alloy with superior corosion resistance over type 430FR solenoid quality but with similar magnetic properties. This datasheet provides information on composition...