Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... CARPENTER 20Mo-6 is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. Its good resistance to corrosion has been...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-556.
Published: 01 July 1999
... Carpenter 20Mo-6 HS is an alloy in the generic family of 6% molybdenum alloys, which are very corrosion resistant. This steel also possesses an excellent resistance to environmental cracking. (See also Carpenter 20Mo-6, Alloy Digest SS-444, May 1984.) This datasheet provides information on...
Journal Articles
Alloy Digest (1995) 44 (8): Ni-484.
Published: 01 August 1995
... corrosion, 20M0-6 stainless should be considered. Potential applications for 20Mo-4 stainless may include heat exchangers, chemical process piping and equipment, mix- ing tanks, and meral cleaning and pickling tanks. II is ex- pected LO find application in flue gas scrubbing systems and in weI process...