Alloy Digest (1994) 43 (7): Ni-458.
Published: 01 July 1994
... Carlson Alloy C601 is characterized by high tensile, yield and creep-rupture strengths for high temperature service. The alloy is not embrittled by extended exposure to high temperatures and has excellent resistance to stress-corrosion cracking, to carburizing, nitriding and sulfur containing...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-463.
Published: 01 September 1994
... Carlson Alloy C400 is a general purpose nickel-copper alloy having an excellent combination of high strength, ductility, weldability and corrosion resistance. It is widely used for handling sulfuric acid under reducing conditions, but also has good resistance to hydrofluoric acid, alkaline...