Alloy Digest (1994) 43 (6): Ni-456.
Published: 01 June 1994
... Carlson Alloys C200 and C201 are wrought forms of nickel with carbon the only difference in composition. The metal has excellent resistance to dry chlorine and hydrogen chloride and caustic alkalis. The alloys combine good mechanical properties with excellent resistance to corrosive environments...