Alloy Digest (2002) 51 (3): SS-846.
Published: 01 March 2002
... Carlson alloys 317L, 317L 4, and 317L 4N are a family of superior corrosion-resistant austenitic stainless steels for service in severe envi-ronments. They maintain tensile and creep-rupture strength at elevated temperatures and are resistant to intergranular attack. These alloys are widely used...