Alloy Digest (1971) 20 (5): SA-265.
Published: 01 May 1971
... USS CARILLOY FC is a resulfurized, medium-carbon, manganese-chromium-molybdenum steel with good machinability and high strength. It is generally furnished in the quenched and tempered condition and requires no further heat treatment. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1957) 6 (1): SA-54.
Published: 01 January 1957
... CARILLOY 2% Cr-1/2% Mo is a low alloy oxidation and corrosion resistant steel suitable for moderately high (900-1100 deg. F.) temperature use. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep...
Journal Articles
Alloy Digest (1959) 8 (9): SA-89.
Published: 01 September 1959
... CARILLOY 1% Cr-1/2% Mo is a low alloy oxidation, corrosion and graphitization resistant steel suitable for moderately high (900-1100 deg. F.) temperature use. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1961) 10 (1): SA-108.
Published: 01 January 1961
... U.S.S. CARILLOY 21/4 Cr-1Mo is a low alloy oxidation and corrosion resistant steel suitable for moderately high (900-1100 F) temperature use. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1955) 4 (1): SA-25.
Published: 01 January 1955
... CARILLOY T-1 is a low-carbon complex alloy steel used where high levels of yield strength and toughness are required. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance...