1-20 of 26 Search Results for

CANNON-MUSKEGON A-2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1973) 22 (6): TS-257.
Published: 01 June 1973
... CANNON-MUSKEGON A-2 is a high-carbon air-hardening cast tool steel with excellent non-deforming properties and abrasion resistance in the quenched and tempered condition. It has good machinability in the annealed condition. A higher silicon content is permissible in this cast steel than in AISI A2...
Journal Articles
Alloy Digest (1973) 22 (7): TS-259.
Published: 01 July 1973
... CANNON-MUSKEGON D-2 is a high-carbon high-chromium air-hardening cast tool steel with excellent resistance to abrasion. It is moderately machinable with excellent non-deforming characteristics. A higher silicon content is permissible in this cast steel than in AISI D2 (wrought) tool steel...
Journal Articles
Alloy Digest (1992) 41 (11): Ni-417.
Published: 01 November 1992
... CMSX-2 is a single crystal alloy development of Cannon-Muskegon Corporation designed to achieve a high level of balanced properties. This datasheet provides information on composition, physical properties, as well ascreep and fatigue. Filing Code: Ni-417. Producer or source: Cannon-Muskegon...
Journal Articles
Alloy Digest (1998) 47 (2): Ni-537.
Published: 01 February 1998
... 1480, and Rene N4. This datasheet provides information on composition and physical properties as well as creep. It also includes information on corrosion resistance as well as casting and heat treating. Filing Code: Ni-537. Producer or source: Cannon-Muskegon Corporation. Producer or Source: Cannon...
Journal Articles
Alloy Digest (1972) 21 (6): TS-244.
Published: 01 June 1972
... tempering cycle should be two (2) hours minimum. Machinability: The machinability rating of the annealed stock of CANNON-MUSKEGON H-19 is about 60% of that of a 1% carbon steel and about 40% of AISI Bll12 steel. Single point turning tools of high speed steel should be ground to 16-20 deg. side rake, 4-7 deg...
Journal Articles
Alloy Digest (1973) 22 (11): SA-296.
Published: 01 November 1973
... CANNON-MUSKEGON 8630 is a medium-carbon triple-alloy cast steel of moderate hardenability. This steel is suitable for many engineering applications and is used in large quantities in the investment casting industry. A higher silicon content is permissible in this steel than in AISI 8630 (wrought...
Journal Articles
Alloy Digest (1978) 27 (5): Ni-255.
Published: 01 May 1978
... CANNON-MUSKEGON Nickel Alloy C is a cast nickel-base alloy with exceptionally high resistance to corrosion and with excellent high-temperature properties. It also has outstanding oxidation resistance and strength at elevated temperatures. Its many uses include heat-treating equipment, aerospace...
Journal Articles
Alloy Digest (1973) 22 (5): TS-255.
Published: 01 May 1973
... CANNON-MUSKEGON H-12 is an air-hardening hot-work cast tool steel used for applications requiring good toughness combined with good red hardness. The alloy will harden from a relatively low austenitizing temperature. A higher silicon content is permissable in this cast steel than in AISI H-12...
Journal Articles
Alloy Digest (1973) 22 (12): SA-299.
Published: 01 December 1973
... CANNON-MUSKEGON 8620 is a low-carbon triple-alloy steel capable of being carburized for wear resistance or heat treated for toughness. This steel is suitable for many engineering applications, and is used in large quantities in the investment casting industry for small parts. A higher silicon...
Journal Articles
Alloy Digest (1993) 42 (1): Ni-420.
Published: 01 January 1993
... CMSX-3 is a single crystal alloy development of Cannon-Muskegon Corporation designed to achieve a balance in properties at high temperatures. This datasheet provides information on composition and physical properties as well as creep. It also includes information on corrosion resistance. Filing...
Journal Articles
Alloy Digest (1973) 22 (3): TS-251.
Published: 01 March 1973
... CANNON-MUSKEGON H-11 is an air-hardening hot-work cast tool steel used for hot applications requiring good toughness combined with good red-hardness and for cold applications where toughness is required at the sacrifice of some wear. A higher silicon content is permissable in this cast steel than...
Journal Articles
Alloy Digest (1972) 21 (8): TS-245.
Published: 01 August 1972
... CANNON-MUSKEGON H-21 is a tough, air-hardening, hot-work tool steel with excellent red hardness and abrasion resistance for high operating temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on casting, heat...
Journal Articles
Alloy Digest (1975) 24 (8): SA-317.
Published: 01 August 1975
... CANNON-MUSKEGON 4140 is a medium-carbon cast alloy steel with good hardenability, strength and toughness. It is used in large quantities in the investment casting industry. A higher silicon content is permissible in this steel than in AISI 4140 (wrought) alloy steel. This datasheet provides...
Journal Articles
Alloy Digest (1994) 43 (3): Ni-447.
Published: 01 March 1994
... dia. (4.8 mm) test bar and .070 dia. (1.8 mm) MFB specimens. See Figure 1. CMSX-2@. CMSX-3@ and Cm 247LC@ are registered made- marks of Cannon-Muskegon Corporation. ...
Journal Articles
Alloy Digest (1992) 41 (12): Ni-418.
Published: 01 December 1992
... alloy development to retrofit existing turbine designs. CMSX-6@ alloy is a registered trademark of Cannon-Muskegon Corporation. Composition, Wt. %: Physical Constants: Chromium 10 Density, lb/cu in. (kg/cu dm) Cobalt 5 Molybdenum 3 Titanium 4.7 Aluminum 4.8 Tantalum 2 Hafnium 0.1 Nickel Bal. PROPERTIES...
Journal Articles
Alloy Digest (1994) 43 (4): Ni-450.
Published: 01 April 1994
... 247LC@. CMSX-2@, CMSX-3@. and CMSX-4 ;ae regis- tered trademarks of Cannon-Muskegon Corporation. MAR M 247@ alloy is a trademark of Martin Marietta Corpora- tion ...
Journal Articles
Alloy Digest (2014) 63 (10): Ni-719.
Published: 01 October 2014
... version of the alloy. This datasheet provides information on composition and tensile properties. It also includes information on casting. Filing Code: Ni-719. Producer or source: Cannon-Muskegon Corporation. Producer or Source: Cannon-Muskegon Corporation Copyright © ASM International® 2014 2014...
Journal Articles
Alloy Digest (2006) 55 (5): Ni-636.
Published: 01 May 2006
...-636. Producer or source: Cannon-Muskegon Corporation. Producer or Source: Cannon-Muskegon Corporation Copyright © ASM International® 2006 2006 ASM International cast nickel alloys castability chemical composition CM 681 LC creep properties physical properties tensile properties...
Journal Articles
Alloy Digest (1968) 17 (8): SS-212.
Published: 01 August 1968
..., physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-212. Producer or source: Cannon-Muskegon Corporation. Producer or Source: Cannon...
Journal Articles
Alloy Digest (1970) 19 (1): Co-60.
Published: 01 January 1970
... properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Co-60. Producer or source: Cannon-Muskegon Corporation. Producer or Source: Cannon-Muskegon Corporation...