Alloy Digest (1972) 21 (3): SS-269.
Published: 01 March 1972
... CA-6NM is a cast stainless steel that has good resistance to cracking during and after solidification of heavy sections, and good weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1196.
Published: 01 January 2015
... Kubota CA-6NM is a hardenable Fe-Cr-Ni-Mo alloy based on the 13% chromium stainless steel alloy CA-15. Ductility, impact properties, and resistance to salt water corrosion are raised by the addition of nickel and molybdenum. Castability in thick or intricate sections is better than that of the 13...
Journal Articles
Alloy Digest (1993) 42 (5): SS-544.
Published: 01 May 1993
... Hardness, Brinell - 255 PROPERTIES ASTM/Grade Table 1 - COMPARATIVE MINIMUM TENSILE PROPERTIES SlMlLAR TENSILE STRENGTH YIELD STRENGTH ELONGATION To ksi MPa ksi Mpa in 2 - % Atlas Alloy 958 CD-4MCu Alloy 255 CA-6NM CF3 CF-3M CG-8M Cw-12Mw - 100 690 75 515 18 - 100 690 70 485 16 - 110 760 70 485 20 - 110...