1-2 of 2 Search Results for

C75S

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2023) 72 (3): CS-242.
Published: 01 March 2023
... 1074, C75S, and S75C are wrought high-carbon (carbon = 0.70–0.80%) non-alloy steels that are, in general, used in the cold worked, quenched and tempered, or austempered condition. These steels are widely used for highly stressed parts that require higher strength levels than can be achieved...
Journal Articles
Alloy Digest (2023) 72 (3): CS-243.
Published: 01 March 2023
... and Processes, Volume 4A, ASM Handbook, ASM International, 2013, p 280 288, httpsdoi.org/10.31399/ asm.hb.v04a.a0005783 22. D. Lober,1.1248 Ck 75 / C75E / C75S, www.metallograf. de 23. J.L. Dossett, Heat Treatment of Carbon and Low-Alloy Steels, Practical Heat Treating Basic Principles, ASM International, 2020...