1-20 of 26 Search Results for

C22

Sort by
Journal Articles
Alloy Digest (2002) 51 (10): Ni-592.
Published: 01 October 2002
... RIMA HAS C22 is a Ni-Cr-Mo-W-type consumable with a nominal composition of Ni, 22% Cr, 13.5% Mo, and 3% W, and it is used to join high-molybdenum-containing corrosion-resistant alloys to themselves and each other by tungsten inert gas (TIG) welding. This datasheet provides information...
Journal Articles
Alloy Digest (2022) 71 (5): CS-222.
Published: 01 May 2022
... 1020, C22, C22E, and C22R are wrought low-carbon non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon...
Journal Articles
Alloy Digest (2023) 72 (10): CS-262.
Published: 01 October 2023
... 1020, C20E2C, and C22 are wrought low-carbon (carbon = 0.17–0.24%) non-alloy steels that are used in the as rolled, normalized, cold worked condition, or quenched and tempered condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can...
Journal Articles
Alloy Digest (2002) 51 (7): Ni-588.
Published: 01 July 2002
...: Nimrod C22KS is an all-positional manual metal arc (MMA) electrode for alloy C22. The electrode has a basic flux with oper- ability optimized for DC+ welding in all positions including fixed pipework qualified in the ASME 5G/6G positions. The electrode is equally suitable for general fabrication welds...
Journal Articles
Alloy Digest (2003) 52 (2): Ni-602.
Published: 01 February 2003
... N06059 DIN 2.4605 (NiCr23Mo16Al) Proprietary Nicrofer 5923hMo (Krupp VDM) Proprietary Inconel alloy 686 (Special Metals) + W Proprietary Hastelloy alloy C2000 (Haynes) + Cu Alloy C22 and similar ASTM/UNS N06022 ASTM/UNS A494 Grade CX2MW (cast) DIN 2.4602 (NiCr21Mo14W) DIN 2.4811, 2.4836 (NiCr20Mo15) DIN...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-596.
Published: 01 December 2002
... (Haynes) + Cu Alloy C22 and similar N06022, A 494 Grade CX2MW (cast) 2.4602 (NiCr21Mo14W), Hastelloy Alloy C22 (Haynes), Nicrofer 5621hMoW (Krupp VDM) 2.4697 (G-NiCr20Mo15) (cast) Superaustenitics S32654, S31254, S34565 654SMO (AvestaPolarit), Uranus B66 (Usinor Industeel) Dissimilar joints between any...
Journal Articles
Alloy Digest (1991) 40 (1): SA-455.
Published: 01 January 1991
...% offset), psi 78000 55000 76000 Elongation (2 in % 20 25 23 Reduction of area, % 42 50 46 Brinell hardness (300 kg) 235 187 235 Rockwell hardness c22 B90 c22 Table 2 - EFFECT OF TEMPERING TEMPERATURE ON RGOM- TEMPERATURE MECHANICAL PROPERTIES - 0.54-m Dia. Bar (Normalized 16OO F, quenched from 1550°F...
Journal Articles
Alloy Digest (1995) 44 (9): SS-610.
Published: 01 September 1995
... as INCONEL@ (a trademark of the INCO fam- ily of companies) 625/112 or HASTELLOY C22@ (HAS- TELLOY and C22 are trademarks of HAYNES Interna- tional Inc.) General Characteristics: URANUS B26 is a 20Cr. 6 MO superaustenitic stainless steel grade with 0.2% nitrogen additions, particularly designed for high...
Journal Articles
Alloy Digest (1996) 45 (11): SS-660.
Published: 01 November 1996
... to maintain the high corrosion resistance of this alloy. Treat simi- larly to other 6 MO superaustenitics for pickling. Weldability: SR 50A can be welded by the following processes: TlG/GTAW, MIG/GMAW. and SMAW with covered electrodes. Typical elec- trodes or filler metal to be used are Alloy C22 or C276...
Journal Articles
Alloy Digest (1973) 22 (9): SA-293.
Published: 01 September 1973
... hardness (300 kg) 235 Rockwell hardness c22 Annealed Normalized 88000 112000 55000 76000 25 23 50 46 187 235 B90 c22 Table 2 - END-QUENCH HARDENABILITY OF 4042H Distance from quenched end, sixteenths of an inch 1 2 4 6 8 IO 12 16 20 24 28 32 Rockwell C hardness, max. 62 60 55 45 36 33 31 29 28 27 27 26...
Journal Articles
Alloy Digest (2022) 71 (9): Ni-781.
Published: 01 September 2022
... Recommendations for Machining See Böhler L022, voestalpine Böhler Edelstahl GmbH, 2001, p 5. Comparable Grades voestalpine Böhler Edelstahl GmbH & Co KG ASTM DIN Trade name Böhler L022 UNS N06022 NiCr21Mo14W (2.4602) Alloy C22 General Characteristics Good ductility; good corrosion resistance; excellent...
Journal Articles
Alloy Digest (1995) 44 (7): SS-602.
Published: 01 July 1995
... of this al- loy. Use 6 MO super-austenitic pickling conditions. Weldability: URANUS B66 can be welded by the following processes: TIG/GTAW, MIG/GMAW, SMAW with covered elec- trodes. Typical electrodes or filler metal to be used are alloy C22 or alloy 59. The weldability is at least equivalent to 6 MO super...
Journal Articles
Alloy Digest (1964) 13 (1): Co-36.
Published: 01 January 1964
..., ft-lbs. (unnotchedj 11 Rockwell hardness c40-44 Table 2 - ELEVATED TEMPERATURE ROCKWELL HARDNESS Test Temperature *Oxy-Acetylene oF Welded Deposit 650 c33 850 c27 1050 c22 1200 c20 1400 A46 *After cooling from test temperatures, the room temperature hard- ness is regained. Heat Treatment: Wallex...
Journal Articles
Alloy Digest (1971) 20 (10): SS-261.
Published: 01 October 1971
... 700 194000 162000 16 900 199000 156000 18 1000 157000 138000 18 1100 137000 121000 19 1200 125000 109000 20 1300 114000 94000 22 1400 101000 79000 26 61 :A 64 64 65 69 72 Rockwell Hardness c43 c43 c43 c34 C28 C25 c22 B99 Table 2 - TYPICAL FATIGUE PROPERTIES Tempering Tensile Fatigue Strength...
Journal Articles
Alloy Digest (2014) 63 (12): SS-1194.
Published: 01 December 2014
... materials like: Phyweld NCW (Nb free 625 for PAW, GTAW, GMAW) ER Ni.Cr.Mo-10 (AWS A5.14) wires and E.Ni.Cr.Mo-10 (AWS A5.11) electrodes (alloy C22 type) EL Ni.Cr.23.Mo-16 or SG-Ni.Cr.23 Mo-16 (DIN 1736) electrodes or filler metal (alloy 59 type can be used Machinability: Contact the producer for data...
Journal Articles
Alloy Digest (1990) 39 (4): SS-304.
Published: 01 April 1990
... - - - - - Anne&&195O F c22 67 - - - >looO >lOOO High-sawlglh (Is). C33 135 - 204 320 >lalO >lOoO l bp.hotrdled c36 144 170L* >looo >lOOO >looo - Cold drawn, 3r8 bnr C41 160 >lOOO - - >lOoO - *LfJnginldiMlspecimesls. NACE TM 01-77 test method. **Ductile creep faihue. Heat Tmatment...
Journal Articles
Alloy Digest (1961) 10 (6): SS-118.
Published: 01 June 1961
...-210000 Yield point, psi 90000-170000 Elongation, % in 2 20-15 Reduction of area, % 65-50 lzod impact, ft. lbs. 70-15 Brine11 Hardness 250-415 Rockwell hardness C22-43 Table 4 - TYPICAL HEAT TREATED PROPERTIES - 1 Bar (Oil quenched from 1750oF. tempered 2 hours) Tensile Yield Reduction Streogth Strength...
Journal Articles
Alloy Digest (2014) 63 (5): Ni-712.
Published: 01 May 2014
... in % Rockwell hardness Heat treated at 1066 °C (1950 °F), rapid quench sheet, 1.27 3.05 (0.050 0.120) Not welded 22 (72) 955 (138.5) 526 (76.3) 53 C22 204 (400) 886 (128.4) 451 (65.4) 50 316 (600) 864 (125.3) 426 (61.8) 49 427 (800) 866 (125.6) 418 (60.6) 51 Sheet and plate, 2.54 8.89 (0.100 0.350) Not welded...
Journal Articles
Alloy Digest (1969) 18 (3): SS-222.
Published: 01 March 1969
... the solution annealed alloy has cooled to room temperature to permit transformation of the austcnite. Normally, transformation is complete in a few hours at room temperature. After transforma- tion. the alloy is magnetic and has a hardness of Rockwell C22-30. Usually, No. 635 is procured from the mill...
Journal Articles
Alloy Digest (1985) 34 (3): SA-408.
Published: 01 March 1985
... UNHARDENED MECHANICAL PROPERTIES - l-in. Dia. Bar Property As-Rolled Annealed Normalized Tensile strength. psi I 15000 86000 I I8000 Yield strength (0.2%, offset). psi 80000 52000 84000 Elongation (2 in 5 ~ 20 25 20 Reduction of area. c r 50 53 51 Brine11 hardness 235 I 70 241 Rockwell hardness c22 B87 C23...