Alloy Digest (2004) 53 (2): SA-436.
Published: 01 February 2004
... Bethlehem Lukens Plate (BLP) C1119/C1144 Modified steels are resulfurized carbon steels containing nominally 1.15% Mn and 0.20 to 0.33% S to provide a free-machining steel. They are recommended especially for high-production automatic machining. They have relatively low hardenability...