1-1 of 1

Search Results for C.D.C. manganese alloy no.720

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1954) 3 (1): Cu-14.
Published: 01 January 1954
... C.D.C. MANGANESE ALLOY No. 720 is a copper-manganese-nickel alloy that responds to hardening by heat treatment. It has high tensile and fatigue strength, wide hardness range, and excellent corrosion resisting characteristics. This datasheet provides information on composition, physical properties...