1-1 of 1 Search Results for

C.D.C. Manganese alloy 780

Sort by
Journal Articles
Alloy Digest (1954) 3 (8): Mn-2.
Published: 01 August 1954
... C.D.C. Manganese Alloy No. 780 is a manganese-copper binary alloy offering unusual combination of properties for power transmission. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes...