Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (12): Cu-158.
Published: 01 December 1965
... Bunting No. 156 is a hard phosphor gear and bearing bronze recommended where the service requirements are severe. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (3): Cu-328.
Published: 01 March 1977
..., but it is attacked with varying degrees of severity if moisture is present in the gas. Specification Equivalents: ASTM B 505, CA 907. SAE: CA 907 (formerly 65). CDA: Copper AIloy No. 907. Federal: QQ-C-390A, CA 907. Note: Bunting Alloy 907 was formerly Bunting Alloy 156. General Characteristics: Bunting alloy 907...