Skip Nav Destination
Close Modal
Search Results for
Brush Alloy M220C
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Brush Alloy M220C
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1966) 15 (7): Ni-114.
Published: 01 July 1966
... Brush Alloy M220C is a betyllium-nickel casting alloy that responds to an age-hardening heat treatment and is characterized by high strength thermal conductivity combined with excellent corrosion, oxidation and wear resistance. It is recommended for mold tooling in the glass industries...
Abstract
View article
PDF
Brush Alloy M220C is a betyllium-nickel casting alloy that responds to an age-hardening heat treatment and is characterized by high strength thermal conductivity combined with excellent corrosion, oxidation and wear resistance. It is recommended for mold tooling in the glass industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-114. Producer or source: Brush Beryllium Company.
Journal Articles
Alloy Digest (1969) 18 (2): Ni-142.
Published: 01 February 1969
... and seizing. Alloy 200C contains alloying additions which provide more strength and structural stability at elevated temperatures than either Brush M220C or Brush 26OC, but at some sacrifice of thermal conductivity. It is recommended for applications re- quiring excellent castabiity, high strength...
Abstract
View article
PDF
BRUSII Alloy 200C is a beryllium-nickel casting alloy having high resistance to wear, corrosion, thermal shock and oxidation. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-142. Producer or source: Brush Beryllium Company.