Alloy Digest (2004) 53 (6): Cu-717.
Published: 01 June 2004
... Brush 60 is a high-performance, lower-priced copper beryllium alloy offering cost-effective solutions for many applications such as electronic contacts and springs in the computer, datacom, and telecommunications markets. It is available in mill-hardened tempers. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-712.
Published: 01 March 2004
... temperatures. Alloy 390 provides excellent stress-relaxation resistance at elevated temperatures, which increases electrical contact reliability. Alloy 390 is a trademark and Brush 60 is a registered trademark of Brush Wellman Inc. Table 1 Alloy Comparisons Yield strength Bend radius, 90° bend, R/t Modulus...
Journal Articles
Alloy Digest (1992) 41 (7): Cu-574.
Published: 01 July 1992
... 200-600 60-180 .002-.OlO .005-.025 125-500 400-150 .002-.OlO .005-.025 The strength, hardness and elongation of Brush Alloy 3C is achieved through age-hardening. The recommended annealing temperature range is 1600-1650°F (860900°C) and the aging temperature is 900°F (480°C). The alloy is typically...
Journal Articles
Alloy Digest (1992) 41 (7): Cu-573.
Published: 01 July 1992
... B50-60 AsCast&Aged 25-45 170-310 55-70 380-480 lo-15 B65-75 Solution Annealed & Aged 70-80 480-550 go-110 620-760 3-15 B92-100 Table 2 - MELTING AND POURING RANGES Solidus Liquidus Pouring Range OF C F C F C Brush Alloy 1OC 1830 1000 1890 1030 2000-2150 1090-1180 DOI: 10.31399/asm.ad.cu0573...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-537.
Published: 01 December 1992
... BRUSH CASTING ALLOYS 275C AND 275CT are beryllium copper alloys of very high strength with cobalt and silicon as the secondary alloying elements. Use is in the age-hardened temper. Brush casting alloy 275CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1987) 36 (12): Cu-532.
Published: 01 December 1987
... BRUSH Alloy 165 has slightly less yield and fatigue strengths than the somewhat higher beryllium-content copper-beryllium alloy. It is cheaper and may be substituted when design requirements are less demanding. It is easily worked to provide complex shapes. This datasheet provides information...
Journal Articles
Alloy Digest (1992) 41 (10): Cu-577.
Published: 01 October 1992
... BRUSH CASTING ALLOYS 245C AND 245CT are beryllium copper (2.25-2.55% Be) alloys of high strength with cobalt as the second alloying element (0.35-0.70% Co). Use is in the age-hardened temper. Brush casting alloy 245CT is the fine-grained version. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1992) 41 (6): Cu-572.
Published: 01 June 1992
... BRUSH 1915 is a heat-treatable leaded copper alloy engineered for automatic screw machining applications when high strength is needed. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on heat treating and machining...
Journal Articles
Alloy Digest (1992) 41 (9): Cu-576.
Published: 01 September 1992
... BRUSH CASTING ALLOYS 165C AND 165CT are beryllium copper alloys of high strength with cobalt as the second alloying element (0.20 to 0.65% Co). Use is in the age-hardened temper. Brush casting alloy 165CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-581.
Published: 01 January 1993
... BRUSH CASTING ALLOYS 20C AND 20CT are beryllium copper alloys (1.90-2.15% Be) of very high strength with cobalt as the second alloying element (0.35 to 0.70% Co). Use is in the age-hardened temper. Brush casting alloy 20CT is the fine-grained version. This datasheet provides information...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-579.
Published: 01 December 1992
... BRUSH chromium copper alloys are heat treatable, corrosion resistant alloys with both high electrical conductivity and strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1986) 35 (10): Cu-516.
Published: 01 October 1986
... BRUSH PHOSPHOR BRONZE is precision rolled and thermally treated to produce a material with consistent formability and properties. The product offers design advantages, improved service life and reduced fabrication problems. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1992) 41 (8): Cu-575.
Published: 01 August 1992
... BRUSH CASTING ALLOY 21C is a beryllium copper alloy of high strength with cobalt as the second alloying element (1.0 to 2.0% Co). Use is in age-hardened temper. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-454.
Published: 01 March 1983
... BRUSH Alloy 3 offers the highest electrical and thermal conductivity of any beryllium-copper alloy. It possesses an excellent combination of moderate strength, good corrosion resistance and good resistance to moderately elevated temperatures. Because of its unique physical and mechanical...
Journal Articles
Alloy Digest (1970) 19 (6): Cu-217.
Published: 01 June 1970
... BRUSH alloy M25 is a free-machining beryllium-copper alloy having good response to age-hardening for high strength, hardness, fatigue and corrosion resistance. It is recommended for screw machine products, gears, shafts, hardware, fasteners, connectors, electronic and electrical components...
Journal Articles
Alloy Digest (1987) 36 (11): Be-7.
Published: 01 November 1987
... BRUSH WELLMAN I-220 is an instrument grade of beryllium strengthened by a dispersion of 2.2% beryllium oxide maximum. It has a micro-yield strength of 5000 psi minimum. I-220B is manufactured from impact ground powder and therefore is more isotropic than BRUSH WELLMAN S-200E. I-220 is often used...
Journal Articles
Alloy Digest (1987) 36 (8): Be-6.
Published: 01 August 1987
... BRUSH WELLMAN I-70A is an instrument and optical grade of beryllium strengthened by a dispersion of 0.7% beryllium oxide maximum. It has relatively low strength and fairly low ductility (a minimum of 2% elongation). Its uses include optical applications, instrumentation, and optical...
Journal Articles
Alloy Digest (1987) 36 (1): Be-3.
Published: 01 January 1987
... BRUSH WELLMAN S-65B is a grade of beryllium strengthened by a dispersion of beryllium oxide. It has moderate strength and fairly low ductility (a minimum of 3% elongation). Its uses include optical applications, nuclear reactors, instrumentation, X-ray windows, high-speed computer parts, audio...
Journal Articles
Alloy Digest (1987) 36 (5): Be-4.
Published: 01 May 1987
... BRUSH WELLMAN S-200F is beryllium strengthened by a dispersion of beryllium oxide (1.5%). It has moderate strength and moderate ductility (A minumum of 2.0% elongation). Its uses include optical equipment, nuclear reactors, instrumentation, optical substrates, satellite structures and solar arrays...
Journal Articles
Alloy Digest (2016) 65 (8): Cu-850.
Published: 01 August 2016
... (40 65) 172 379 (25 55) 1 20 HT 0.76 11.1 (0.030 0.4375) 552 724 (80 105) 483 655 (70 95) 4 30 >11.1 15.9 (>0.4375 0.625) 483 689 (70 100) 345 586 (55 85) 4 30 Brush 1916 wire A 0.76 15.9 (0.030 0.625) 138 345 (20 50) 34 172 (5 25) 40 60 AT 0.76 15.9 (0.030 0.625) 345 483 (50 70) 172 345 (25 50) 25 45...