Alloy Digest (1961) 10 (12): Cu-111.
Published: 01 December 1961
... Bridgeport Alloy 77 is a modified copper-zinc brass having improved resistance to bio-fouling, dezincification, and other forms of copper attack. It is recommended for condenser and heat exchanger tubes for marine use. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1966) 15 (3): Cu-162.
Published: 01 March 1966
... Bridgeport Alloy 520 is a copper-nickel alloy recommended for applications wherever impingement, general corrosion or erosion is severe or its properties at elevated temperatures are desired. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1964) 13 (5): Cu-141.
Published: 01 May 1964
... Bridgeport 54 is a copper-zinc-aluminum alloy having high corrosion and erosion resistance combined with good strength and ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1956) 5 (12): Cu-45.
Published: 01 December 1956
... treating, machining, joining, and surface treatment. Filing Code: Cu-45. Producer or source: Bridgeport Brass Company. Producer or Source: Bridgeport Brass Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys Duronze 609...
Journal Articles
Alloy Digest (1964) 13 (2): Cu-138.
Published: 01 February 1964
... as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-138. Producer or source: Bridgeport Brass Company. Producer or Source: Bridgeport Brass Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys...
Journal Articles
Alloy Digest (1959) 8 (1): Cu-71.
Published: 01 January 1959
... as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-71. Producer or source: Bridgeport Brass Company. Producer or Source: Bridgeport Brass Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys...