Publisher: Journals Gateway
Alloy Digest (1964) 13 (11): Ag-3.
Published: 01 November 1964
... BRAZE 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. This datasheet provides information on composition and physical properties. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (11): Cu-362.
Published: 01 November 1978
... also must be large to provide ample feeding of the sections. Casting methods include centrifugal, contin- uous, ingot and sand. Joinability: Copper Alloy No. 852 has an excellent response to soft soldering. It also exhibits good brazing characteristics. It has fair performance in the butt-type...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (10): Cu-852.
Published: 01 October 2016
... soldering, brazing, cold working, and plating characteristics. Forgeability is rated as 65% of C37700 (forging brass). Weldability: Soldering and brazing are excellent, oxyacetylene welding is fair, and arc welding is good. However, coated metal arc welding, spot welding, and seam welds are not recommended...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (11): Al-248.
Published: 01 November 1983
... tendency and pressure tightness) are inferior 10 those of many other aluminum casting alloys. Good foundry techniques and special care are recommended. Joinability: Aluminum 852.0 has poor suitability for joining by welding and normally is not fabricated by welding. Joining by brazing is not recommended...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (7): Cu-77.
Published: 01 July 1959
... timing, short time-on periods, and lower electrode pressure and higher current than for steel of comparable thickness. Manufacturer: Brazing and Soldering: Silver-alloy brazing and soldering are easily done. Corrosion Resistance: This alloy o&s excellent resistance to corrosion by fresh water, sea water...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (4): Cu-435.
Published: 01 April 1982
... and therefore is suitable for coining, deep drawing, stamping and spinning. It is coined in the annealed tempers shown in Table 1. Joinability: Copper Alloy No. C71300 has excellent suitability for joining by soldering or brazing. It also has excel- lent suitability for gas-shielded arc welding and for spot...